Effect of Thermal Cycling on Abrasive Wear Response of Cu-1.9Be-0.25(Co+Ni) Alloy

Cu-Be alloys are considered high strength alloys when containing 0.2% to 2% of Be per weight, 0.2% to 2.7% of Co per weight, and up to 2.2% of Ni per weight, since they can present an elastic limit higher than 1380 MPa after aging (precipitation hardening), while, without heat treatment, they presen...

Descrizione completa

Dettagli Bibliografici
Autori principali: Higuera-Cobos, Oscar Fabián, Moreno-Téllez, Carlos Mauricio, Pedraza-Yepes, Cristian Antonio
Natura: Online
Lingua:eng
Pubblicazione: Universidad Pedagógica y Tecnológica de Colombia 2020