The dehydration process of two limonitic ores from Venezuela was studied between 250 °C and 950 °C by means of thermogravimetry, infrared spectroscopy, and x-ray diffraction. These techniques indicated for both minerals that the goethite-to-hematite transformation occurred in the range of 250-350 °C...